PCBN / HARD TURNING
PCBN 牌号
以可控、可重复的硬车削替代 45–65 HRC 钢件磨削。
| Grade | CBN / 涂层 | 硬度 | 结合剂 | TRS | 耐温 | 应用 |
|---|---|---|---|---|---|---|
| OK-PCBN 50 | 50% CBN / TiN | 3,200 HV | Ceramic | 1,000 MPa | 1,200 °C | Hardened steel, continuous cut |
| OK-PCBN 70 | 70% CBN / TiAlN | 3,800 HV | Ceramic | 900 MPa | 1,200 °C | Interrupted cuts, powder metal |
| OK-PCBN 90 | 90% CBN / Al | 4,300 HV | Aluminium | 800 MPa | 1,300 °C | High-hardness white cast iron |
PCD / NON-FERROUS
PCD 牌号
铝、铜与金属基复合材料的高速镜面加工。
| Grade | 粒度 / 结合 | 硬度 | 结合剂 | TRS | 耐温 | 应用 |
|---|---|---|---|---|---|---|
| OK-PCD 10 | 10 µm / Co | 8,500 HV | Cobalt | 1,350 MPa | 700 °C | Aluminium alloys, copper |
| OK-PCD 25 | 25 µm / Co | 9,200 HV | Cobalt | 1,250 MPa | 700 °C | MMC, CFRP, abrasive polymers |
| OK-PCD 05 | 5 µm / Co | 8,000 HV | Cobalt | 1,450 MPa | 700 °C | Mirror finishing, copper |
典型起始参数
| D2 / 62 HRC | 120–200 m/min | 0.08–0.15 mm/rev | 0.2–0.5 mm |
| AlSi10Mg | 500–1,200 m/min | 0.05–0.20 mm/rev | 0.1–0.4 mm |
| CFRP | 200–400 m/min | 0.05–0.15 mm/rev | 0.1–0.3 mm |
| 白口铸铁 | 60–120 m/min | 0.08–0.15 mm/rev | 0.2–0.6 mm |
仅作起始值,不代表保证寿命。必须按机床、夹具和工件试切。
刃口与公差
- 典型尺寸公差
- ±0.005 mm
- 刃口处理
- Chamfer + hone, wiper
- 表面粗糙度
- Ra 0.35–0.8 µm
- 首件报告
- CMM + edge photos
- 批次追溯
- Powder lot → sinter → edge