SELECTION REFERENCE
Superhard tooling. Written as data.
PCBN and PCD grades, hardness, starting parameters, edge preparation and tolerance. Final values are confirmed by workpiece, drawing and machine.
PCBN / HARD TURNING
PCBN grades
Replace grinding on 45–65 HRC steel with a controlled, repeatable hard-turning process.
| Grade | CBN / coating | Hardness | Binder | TRS | Temp. | Application |
|---|---|---|---|---|---|---|
| OK-PCBN 50 | 50% CBN / TiN | 3,200 HV | Ceramic | 1,000 MPa | 1,200 °C | Hardened steel, continuous cut |
| OK-PCBN 70 | 70% CBN / TiAlN | 3,800 HV | Ceramic | 900 MPa | 1,200 °C | Interrupted cuts, powder metal |
| OK-PCBN 90 | 90% CBN / Al | 4,300 HV | Aluminium | 800 MPa | 1,300 °C | High-hardness white cast iron |
PCD / NON-FERROUS
PCD grades
Mirror finishes in aluminium, copper and metal-matrix composites — at production speeds.
| Grade | Grain / bond | Hardness | Binder | TRS | Temp. | Application |
|---|---|---|---|---|---|---|
| OK-PCD 10 | 10 µm / Co | 8,500 HV | Cobalt | 1,350 MPa | 700 °C | Aluminium alloys, copper |
| OK-PCD 25 | 25 µm / Co | 9,200 HV | Cobalt | 1,250 MPa | 700 °C | MMC, CFRP, abrasive polymers |
| OK-PCD 05 | 5 µm / Co | 8,000 HV | Cobalt | 1,450 MPa | 700 °C | Mirror finishing, copper |
Starting parameters
| D2 / 62 HRC | 120–200 m/min | 0.08–0.15 mm/rev | 0.2–0.5 mm |
| AlSi10Mg | 500–1,200 m/min | 0.05–0.20 mm/rev | 0.1–0.4 mm |
| CFRP | 200–400 m/min | 0.05–0.15 mm/rev | 0.1–0.3 mm |
| White cast iron | 60–120 m/min | 0.08–0.15 mm/rev | 0.2–0.6 mm |
Starting values only; not a guaranteed tool life. Prove out on the machine, fixture and workpiece.
Edge & tolerance
- Typical tolerance
- ±0.005 mm
- Edge prep
- Chamfer + hone, wiper
- Surface finish
- Ra 0.35–0.8 µm
- First article
- CMM + edge photos
- Traceability
- Powder lot → sinter → edge
Need a grade recommendation for your workpiece? Send the drawing, material, hardness, machine and target life.
Send a drawing →